Exploring the stress-corrosion cracking susceptibility of additively manufactured 316L in boiling magnesium chloride

Karasz, Erin K.; Taylor, Jason M.; Autenrieth, David; Reu, P.L.; Johnson, Kyle L.; Melia, Michael A.; Noell, Philip