Publications Details

Publications / Conference Presentation

Understanding The Exceptional Chloride-induced Stress Corrosion Cracking Resistance Of Stainless Steel 304L Cold Spray Coating

Qu, Haozheng; Schindelholz, Eric; Marino, Gabriella; Locke, Jenifer; Schaller, Rebecca S.; Wharry, Janelle

Abstract not provided.