Pit-to-Crack Transition in Stress Corrosion Cracking of Type 304 Stainless Steels Under Marine Exposure Conditions

Parey, Alana; Schaller, Rebecca S.; Srinivasan, Jay; Locke, Jenifer; Schindelholz, Eric