Development of a consistent geochemical model of the Mg(OH)2–MgCl2–H2O system from 25°C to 120°C

Applied Geochemistry

Knight, Andrew W.; Bryan, Charles R.; Jove Colon, Carlos F.

The formation of magnesium chloride-hydroxide salts (magnesium hydroxychlorides) has implications for many geochemical processes and technical applications. For this reason, a thermodynamic database for evaluating the Mg(OH)2–MgCl2–H2O ternary system from 0 °C–120 °C has been developed based on extensive experimental solubility data. Internally consistent sets of standard thermodynamic parameters (ΔGf°, ΔHf°, S°, and CP) were derived for several solid phases: 3 Mg(OH)2:MgCl2:8H2O, 9 Mg(OH)2:MgCl2:4H2O, 2 Mg(OH)2:MgCl2:4H2O, 2 Mg(OH)2:MgCl2: 2H2O(s), brucite (Mg(OH)2), bischofite (MgCl2:6H2O), and MgCl2:4H2O. First, estimated values for the thermodynamic parameters were derived using a component addition method. These parameters were combined with standard thermodynamic data for Mg2+(aq) consistent with CODATA (Cox et al., 1989) to generate temperature-dependent Gibbs energies for the dissolution reactions of the solid phases. These data, in combination with values for MgOH+(aq) updated to be consistent with Mg2+-CODATA, were used to compute equilibrium constants and incorporated into a Pitzer thermodynamic database for concentrated electrolyte solutions. Phase solubility diagrams were constructed as a function of temperature and magnesium chloride concentration for comparisons with available experimental data. To improve the fits to the experimental data, reaction equilibrium constants for the Mg-bearing mineral phases, the binary Pitzer parameters for the MgOH+ — Cl− interaction, and the temperature-dependent coefficients for those Pitzer parameters were constrained by experimental phase boundaries and to match phase solubilities. These parameter adjustments resulted in an updated set of standard thermodynamic data and associated temperature-dependent functions. The resulting database has direct applications to investigations of magnesia cement formation and leaching, chemical barrier interactions related to disposition of heat-generating nuclear waste, and evaluation of magnesium-rich salt and brine stabilities at elevated temperatures.

More Details

Towards understanding stress corrosion cracking of austenitic stainless steels exposed to realistic sea salt brines

Corrosion Science

Katona, Ryan M.; Taylor, Jason M.; Mccready, T.A.; Bryan, Charles R.; Schaller, Rebecca S.

Stress corrosion cracking behavior of stainless steel 304 L was investigated in full immersion, evaporated artificial sea salt brines (ASW) at 55 °C. It was observed that brines representative of thermodynamically stable brines at lower relative humidity (40% RH, MgCl2-dominant) had a faster crack growth rate than high relative humidity brines (76% RH, NaCl-dominant). Observed crack growth rates (da/dt) under constant stress intensity (K) conditions were determined to be independent of transitioning procedure (rising K or decreasing frequency) regardless of solutions investigated for the orientation presented. Further, positive strain rates had little to no impact on the observed da/dt. The observed behavior suggests an anodic dissolution enhanced hydrogen embrittlement mechanism for SS304L in concentrated ASW environments at 55 °C. Additional explorations further examined environmental influences on da/dt. Nitrate additions to 40% ASW at 55 °C solutions were shown to decrease measured da/dt and further additions stopped measurable crack growth. After sufficient nitrate had been added to fully stifle crack growth, a temperature increase to 75 °C induced cracking again, and a subsequent decrease to 55 °C once again stopped da/dt. These tests demonstrate the importance of ascertaining both brine-specific chemical and dynamic environmental influences on da/dt.

More Details

FY23 Status Report: SNF Interim Storage Canister Corrosion and Surface Environment Investigations

Bryan, Charles R.; Knight, Andrew W.; Katona, Ryan M.; Smith, Elizabeth; Schaller, Rebecca S.

Work evaluating spent nuclear fuel (SNF) dry storage canister surface environments and canister corrosion progressed significantly in FY23, with the goal of developing a scientific understanding of the processes controlling initiation and growth of stress corrosion cracking (SCC) cracks in stainless steel canisters in relevant storage environments. The results of the work performed at Sandia National Laboratories (SNL) will guide future work and will contribute to the development of better tools for predicting potential canister penetration by SCC.

More Details

Corrosion-Resistant Coatings on Spent Nuclear Fuel Canisters to Mitigate and Repair Potential Stress Corrosion Cracking (FY23 Status)

Nation, Brendan L.; Knight, Andrew W.; Maguire, Makeila M.; Verma, Samay; Click, Natalie; Debrun, Gavin; Mccready, T.A.; Katona, Ryan M.; Schaller, Rebecca S.; Bryan, Charles R.

This report summarizes the activities performed by Sandia National Laboratories in FY23 to identify and test coating materials for the prevention, mitigation, and/or repair of potential chloride-induced stress corrosion cracking in spent nuclear fuel dry storage canisters. This work continues efforts by Sandia National Laboratories that are summarized in previous reports from FY20 through FY22 on the same topic. In FY23, Sandia National Laboratories, in collaboration with five industry partners through a memorandum of understanding, evaluated the physical, mechanical, and corrosion-resistance properties of eight different coating systems. The evaluation included thermal and radiation environments relevant to various time periods of storage for spent nuclear fuel canisters. The coating systems include polymeric (polyetherketoneketone, modified polyimide/polyurea, modified phenolic resin, epoxy), organic/inorganic ceramic hybrids (silane-based polyurethane hybrid and a quasi-ceramic sol-gel polyurethane hybrid), and coatings utilizing a Zn-rich primer applied to stainless steel coupons. The results and implications of these tests are summarized in this report. These analyses will be used to identify the most effective coatings for potential use on spent nuclear fuel dry storage canisters and to identify specific needs for further optimization of coating technologies for application on spent nuclear fuel canisters.

More Details

Considerations for realistic atmospheric environments: An application to corrosion testing

Science of the Total Environment

Katona, Ryan M.; Knight, Andrew W.; Maguire, Makeila M.; Bryan, Charles R.; Schaller, Rebecca S.

Measured salt compositions in dust collected over roughly the last decade from surfaces of in-service stainless-steel alloys at four locations around the United States are presented, along with the predicted brine compositions that would result from deliquescence of these salts. The salt compositions vary greatly from ASTM seawater and from laboratory salts (i.e., NaCl or MgCl2) commonly used on corrosion testing. The salts contained relatively high amounts of sulfates and nitrates, evolved to basic pH values, and exhibited deliquescence relative humidity values (RH) higher than seawater. Additionally, inert dust in components were quantified and considerations for laboratory testing are presented. The observed dust compositions are discussed in terms of the potential corrosion behavior and are compared to commonly used accelerated testing protocols. Finally, ambient weather conditions and their influence on diurnal fluctuations in temperature (T) and RH on heated metal surfaces are evaluated and a relevant diurnal cycle for laboratory testing a heated surface has been developed. Suggestions for future accelerated tests are proposed that include exploration of the effects of inert dust particles on atmospheric corrosion, chemistry considerations, and realistic diurnal fluctuations in T and RH. Understanding mechanisms in both realistic and accelerated environments will allow development of a corrosion factor (i.e., scaling factor) for the extrapolation of laboratory-scale test results to real world applications.

More Details

Influence of Realistic, Cyclic Atmospheric Cycles on the Pitting Corrosion of Austenitic Stainless Steels

Journal of the Electrochemical Society

Schaller, Rebecca S.; Karasz, Erin K.; Bryan, Charles R.; Snow, J.; Taylor, Jason M.; Kelly, R.G.; Montoya, T.

Pitting corrosion was evaluated on stainless steels 304H, 304, and 316L the surfaces of which had ASTM seawater printed on them as a function of surface roughness after exposure to an exemplar realistic atmospheric diurnal cycle for up to one year. Methods to evaluate pitting damage included optical imaging, scanning electron microscopy imaging, profilometry analysis, and polarization scans. The developed cyclic exposure environment did not significantly influence pitting morphology nor depth in comparison to prior static exposure environments. Cross-hatching was observed in a majority of pits for all material compositions with the roughest surface finish (#4 finish) and in all surface finishes for the 304H composition. Evidence is provided that cross-hatched pit morphologies are caused by slip bands produced during the grinding process for the #4 finish or by material processing. Additionally, micro-cracking was observed in pits formed on samples with the #4 surface finish and was greatly reduced or absent for pits formed on samples with smooth surface finishes. This suggests that both a low RH leading to an MgCl2-dominated environment and a rough surface containing significant residual stress are necessary for micro-cracking. Finally, the use of various characterization techniques and cross sectioning was employed to both qualitatively and quantitatively assess pitting damage across all SS compositions and surface finishes.

More Details

Corrosion-Resistant Coatings on Spent Nuclear Fuel Canisters to Mitigate and Repair Potential Stress Corrosion Cracking (FY22 Status)

Knight, Andrew W.; Nation, Brendan L.; Maguire, Makeila M.; Schaller, Rebecca S.; Bryan, Charles R.

This report summarizes the activities performed by Sandia National Laboratories in FY22 to identify and test coating materials for the prevention, mitigation, and/or repair of potential chloride-induced stress corrosion cracking in spent nuclear fuel dry storage canisters. This work continues efforts by Sandia National Laboratories that are summarized in previous reports in FY20 and FY21 on the same topic. The previous work detailed the specific coating properties desired for application and implementation to spent nuclear fuel canisters (FY20) and identified several potential coatings for evaluation (FY21). In FY22, Sandia National Laboratories, in collaboration with four industry partners through a Memorandum of Understanding, started evaluating the physical, mechanical, and corrosion-resistance properties of 6 different coating systems (11 total coating variants) to develop a baseline understanding of the viability of each coating type for use to prevent, mitigate, and/or repair potential stress corrosion on cracking on spent nuclear fuel canisters. This collaborative R&D program leverages the analytical and laboratory capabilities at Sandia National Laboratories and the material design and synthesis capabilities of the industry collaborators. The coating systems include organic (polyetherketoneketone, modified polyimide/polyurea, modified phenolic resin), organic/inorganic ceramic hybrids (silane-based polyurethane hybrid and a quasi-ceramic sol-gel polyurethane hybrid), and hybrid systems in conjuncture with a Zn-rich primer. These coatings were applied to stainless steel coupons (the same coupons were supplied to all vendors by SNL for direct comparison) and have undergone several physical, mechanical, and electrochemical tests. The results and implications of these tests are summarized in this report. These analyses will be used to identify the most effective coatings for potential use on spent nuclear fuel dry storage canisters, and also to identify specific needs for further optimization of coating technologies for their application on spent nuclear fuel canisters. In FY22, Sandia National Laboratories performed baseline testing and atmospheric exposure tests of the coating samples supplied by the vendors in accordance with the scope of work defined in the Memorandum of Understanding. In FY23, Sandia National Laboratories will continue evaluating coating performance with a focus on thermal and radiolytic stability.

More Details

Analysis of Dust Samples Collected from a Near-Marine East Coast ISFSI Site ("Site C")

Bryan, Charles R.; Knight, Andrew W.; Maguire, Makeila M.

In June of 2022, dust samples were collected from the surface of an in-service spent nuclear fuel dry storage canister during an inspection at an Independent Spent Fuel Storage Installation. The site is anonymous but is a near-marine or brackish water east coast location referred to here as "Site C". The purpose of the sampling was to assess the composition and abundance of the soluble salts present on the canister surface, information that provides a metric for potential corrosion risks. Following collection, the samples were delivered to Sandia National Laboratories for analysis. At Sandia, the soluble salts were leached from the dust and quantified by ion chromatography. In addition, subsamples of the dust were taken for scanning electron microscopy to determine the particle sizes, morphology, and mineralogy of the dust and salts. The results of those analyses are presented in this report.

More Details

FY2022 Status Update: A Probabilistic Model for Stress Corrosion Cracking of SNF Dry Storage Canisters

Gilkey, Lindsay N.; Brooks, Dusty M.; Katona, Ryan M.; Bryan, Charles R.; Schaller, Rebecca S.

Understanding the potential risk of stress corrosion cracking of spent nuclear fuel dry storage canisters has been identified as a knowledge gap for determining the safety of long-term interim storage of spent nuclear fuel. To address this, the DOE is funding a multi-lab DOE effort to understand the timing, occurrence, and consequences of potential canister SCC. Sandia National Laboratories has developed a probabilistic model for canister penetration by SCC. This model has been continuously updated at SNL since 2014. Model uncertainties are treated using a nested loop structure, where the outer loop accounts for uncertainties due to lack of data and the inner aleatoric loop accounts for uncertainties due to variation in nature. By separating uncertainties into these categories, it is possible to focus future work on reducing the most influential epistemic uncertainties. Several experimental studies have already been performed to improve the modeling approach through expanded process understanding and improved model parameterization. The resulting code is physics-based and intended to inform future work by identifying (1) important modeling assumptions, (2) experimental data needs, and (3) necessary model developments. In this document, several of the sub-models in the probabilistic SCC model have been exercised, and the intermediate results, as the model progresses from one sub-model to the next, are presented. Evaluating the sub-models in this manner provides a better understanding of sub-model outputs and has identified several unintended consequences of model assumptions or parameterizations, requiring updates to the modeling approach. The following updates have been made, and future updates have been identified.

More Details

Physical and chemical properties of sea salt deliquescent brines as a function of temperature and relative humidity

Science of the Total Environment

Katona, Ryan M.; Bryan, Charles R.; Knight, Andrew W.; Sanchez, Amanda C.; Schindelholz, E.J.; Schaller, Rebecca S.

Thermodynamic modeling has been used to predict chemical compositions of brines formed by the deliquescence of sea salt aerosols. Representative brines have been mixed, and physical and chemical properties have been measured over a range of temperatures. Brine properties are discussed in terms of atmospheric corrosion of austenitic stainless steel, using spent nuclear fuel dry storage canisters as an example. After initial loading with spent fuel, during dry storage, the canisters cool over time, leading to increased surface relative humidities and evolving brine chemistries and properties. These parameters affect corrosion kinetics and damage distributions, and may offer important constraints on the expected timing, rate, and long-term impacts of canister corrosion.

More Details

Development of Surface Sampling Techniques for the Canister Deposition Field Demonstration (FY22 Update)

Knight, Andrew W.; Schaller, Rebecca S.; Nation, Brendan L.; Durbin, S.G.; Bryan, Charles R.

This report describes the proposed surface sampling techniques and plan for the multi-year Canister Deposition Field Demonstration (CDFD). The CDFD is primarily a dust deposition test that will use three commercial 32PTH2 NUHOMS welded stainless steel storage canisters in Advanced Horizontal Storage Modules, with planned exposure testing for up to 10 years at an operating ISFSI site. One canister will be left at ambient condition, unheated; the other two will have heaters to achieve canister surface temperatures that match, to the degree possible, spent nuclear fuel (SNF) loaded canisters with heat loads of 10 kW and 40 kW. Surface sampling campaigns for dust analysis will take place on a yearly or bi-yearly basis. The goal of the planned dust sampling and analysis is to determine important environmental parameters that impact the potential occurrence of stress corrosion cracking on SNF dry storage canisters. Specifically, measured dust deposition rates and deposited particle sizes will improve parameterization of dust deposition models employed to predict the potential occurrence and timing of stress corrosion cracks on the stainless steel SNF canisters. The size, morphology, and composition of the deposited dust and salt particles will be quantified, as well as the soluble salt load per unit area and the rate of deposition, as a function of canister surface temperature, location, time, and orientation. Previously, a preliminary sampling plan was developed, identifying possible sampling locations on the canister surfaces and sampling intervals; possible sampling methods were also described. Further development of the sampling plan has commenced through three different tasks. First, canister surface roughness, a potentially important parameter for air flow and dust deposition, was characterized at several locations on one of the test canisters. Second, corrosion testing to evaluate the potential lifetime and aging of thermocouple wires, spot welds, and attachments was initiated. Third, hand sampling protocols were developed, and initial testing was carried out. The results of those efforts are presented in this report. The information obtained from the CDFD will be critical for ongoing efforts to develop a detailed understanding of the potential for stress corrosion cracking of SNF dry storage canisters.